RubberTypical Values | Standard | FRAS | Reference Standard |
Tensile Strength / MPa | 20 | 16 | GB/T 528-2009 |
Elongation at Break/% | 600% | 550% | GB/T 528-2009 |
Hardness/Shore A | 63±5 | 63±5 | GB/T 531.1 |
Abrasion Loss/mm3 | 110 | 150 | GB/T 9867 |
Aging Test | Tensile Strength+ 1.0% Elongation at Break -8.3% | Tensile Strength+0.3 % Elongationat Break-3.3% |
GB/T3512 |
Visible Flame Duration / s | N/A | 1 | MT/T113 |
Visible Afterglow Duration / s | N/A | 80 | MT/T113 |
Electrical Resistance(Surface)/Q | N/A | 3x104 | MT/T113 |
Continuous Operating Temperature^ | -40°C~80°C | -40°C-80°C | |
Peel Strength / MPa | 13 | 13 | GB/T 15254 |